Material Selection for Automobile Wiper Plastic Part Injection Mold
Automobile wiper plastic parts work in harsh outdoor environments, enduring rain, ultraviolet radiation, high and low temperature cycles and repeated fatigue load from swinging. Some structural parts are squeezed and rubbed by metal shafts. Material selection at the early mold development stage directly determines weather resistance, assembly precision and service life. The wiper assembly includes connecting rod sleeves, base, arm cover, rubber buckle and gear seat. Materials are selected according to stress and environmental conditions of different positions, balancing molding performance and mass production cost.
Working Conditions and Core Selection Indicators of Wiper Plastic Parts
Core evaluation indicators include UV aging resistance, low-temperature toughness, hydrolysis resistance, friction and wear, dimensional stability and chemical corrosion resistance. The surface temperature can reach above 80℃ in summer and drop below -30℃ in winter. Materials should not crack, whiten or deform under temperature cycles. Splash of car wash liquid, antifreeze, oil and salt spray will erode plastic surfaces and cause cracking and peeling. Friction parts need low friction coefficient to reduce abnormal noise and wear. Appearance parts need stable color to prevent yellowing and fading. Modified engineering plastics are the mainstream choice, as general plastics cannot meet all these requirements.

Material Matching Scheme for Different Wiper Components
ASA is the first choice for appearance parts such as wiper arm covers and decorative housings. Without butadiene double bonds vulnerable to UV attack, ASA is resistant to yellowing and pulverization after long-term outdoor exposure, with stable coloring and good fluidity for uniform matte texture. ABS mixed with weather-resistant additives is a low-cost alternative for low-end models with shorter aging cycle. TPE or TPV is used for flexible protective parts including connecting rod sleeves, ball joint dust covers and gaskets. They have good elasticity and low compression set, closely fitting metal ball joints to block mud and water. TPV has better oil and weather resistance than ordinary TPE and is preferred by OEMs. Glass fiber reinforced PA66 is widely used for load-bearing structural parts such as transmission supports and gear bases. Glass fiber improves rigidity, tensile strength and dimensional stability, resisting creep under long-term alternating load. Hydrolysis-resistant toughened PA66 is used for cold regions to avoid low-temperature impact fracture. POM is adopted for small wear-resistant gears and sliding bushes with low friction coefficient and self-lubricating property. But POM has poor weather resistance and can only be used in shaded internal positions. PBT is used for locking buckles and high-strength connectors of high-end wipers, featuring fast molding speed, stable shrinkage and excellent chemical resistance.

Molding Matching and Mold Adaptation Points
Mold design should match raw material characteristics after material selection. Glass fiber reinforced PA66 and PBT cause heavy mold wear, so S136 or nitrided 718H is adopted for cavity, sliding blocks and inserts. POM releases acidic decomposition gas during molding, so anti-rust steel is required and vent grooves are reasonably arranged to avoid cavity corrosion and product burning. ASA appearance parts require high polishing and texture quality. Gates are arranged away from appearance surfaces to control shear heat and reduce color difference and flow marks. For TPE and TPV overmolding, substrate polarity should be matched and draft angle controlled to avoid whitening during demolding. Raw materials such as PA66 and PBT must be fully dried to eliminate bubbles and silver streaks caused by moisture. Toughened modified materials are sensitive to shear, so screw speed and back pressure should be controlled to avoid molecular chain breakage and toughness decline.
Common Selection Misunderstandings and Verification Requirements
Many projects only focus on rigidity and ignore weather resistance tests, resulting in yellowing and cracking after half a year on vehicles. Ordinary ABS cannot replace ASA for appearance parts, as defects will appear after UV aging. High hardness alone cannot solve abnormal noise of friction parts without self-lubricating structure. After material selection, samples must pass xenon lamp aging, high-low temperature impact, salt spray and liquid immersion tests to verify strength and elongation changes after aging and meet vehicle durability standards. Material selection for wiper plastic parts is a balance of weather resistance, mechanical property, friction performance and cost. Parts are classified as exposed appearance parts, internal load-bearing parts or flexible sealing parts for targeted selection, to ensure stable operation of wiper systems and reduce after-sales faults such as abnormal noise and fracture.