Common problem

Flame Retardancy and Insulation Requirements of China Power Battery Pack Housing Injection Molded Parts

2026-11-26 11:35:26 Injection Molding

Power battery pack housings serve as critical protective structures for battery systems, which function to isolate battery cells, block heat propagation and provide high-voltage insulation. Failure in flame retardancy or insulation performance may lead to electric leakage and thermal runaway risks. Material selection, molding process control and finished product testing must comply with relevant standards to achieve long-term safety stability.

1. Flame Retardancy Grades and Relevant Standards

The UL94 standard is widely adopted for power battery plastic components. Most projects require V-0 grade, while parts located in high-voltage zones may demand 5VA grade. Different from ordinary household flame-retardant plastics, battery-grade formulas prefer halogen-free, low-smoke and low-toxicity systems. Halogen-containing flame retardants release corrosive gas under high temperature and damage surrounding wiring and metal terminals. It is important to note that raw material certificates cannot represent the final performance of molded products. Excessive shearing heat, overhigh barrel temperature and uncontrolled regrind ratio will decompose flame retardant additives and downgrade flame retardant performance. The UL yellow card must be checked against the actual wall thickness, since a material reaching V-0 at 3 mm may only achieve V-1 at 1.5 mm. Meanwhile, the design needs to meet GB 38031, which regulates the thermal runaway resistance of traction batteries.

injection mould

2. Control of Insulation Performance Indicators

Core insulation indicators include insulation resistance, breakdown voltage and CTI. CTI value for high-voltage battery pack parts is generally required above 600 V. Materials with low CTI are prone to tracking leakage under condensation and dust accumulation. High water absorption materials will suffer continuous insulation attenuation in humid environments, so low-water-absorption modified PP, PC/ABS and PPS are preferred. Structural design should reserve sufficient electrical clearance and creepage distance. Narrow gaps and grooves need to be avoided to reduce dust and moisture accumulation. Conductive impurities such as metal debris and excessive carbon black must be strictly blocked during production, as these impurities will directly destroy insulation performance.

3. Material System Selection Guidelines

Modified halogen-free flame-retardant PP is commonly used for lower housings and protective covers, featuring low density and cost advantages, while its temperature resistance and creep resistance are limited. Flame-retardant PC/ABS has outstanding toughness and impact resistance, suitable for upper covers and wiring brackets. High-temperature engineering plastics such as PPS and PPA are applied to high-voltage isolation brackets, with stable dimensional performance and high CTI value. Glass-fiber reinforced materials can improve rigidity, but floating fiber on the surface will reduce tracking resistance. The compatibility of additives should be verified, because precipitated additives may form conductive films on the surface.

4. Influence of Mold and Molding Process on Flame Retardancy and Insulation

Flame-retardant plastics are sensitive to heat. Excessive screw speed, back pressure and melt temperature will decompose flame retardants and generate carbon deposits on the cavity surface. The proportion of regrind is usually limited below 10%, and some OEMs prohibit regrind completely. Adequate venting is required to exhaust decomposed gas and prevent scorch and bubbles. Hot runner systems are recommended for long-flow parts to reduce shear heat and material degradation. Stable mold temperature helps reduce internal stress, which prevents cracking under alternating cold and hot conditions.

injection mould

5. Finished Product Testing and Aging Verification

Samples need to pass flame test, breakdown voltage test, insulation resistance test and CTI test. Environmental aging tests including temperature cycling, damp heat and salt spray are mandatory. Damp heat aging is the key test item, as many qualified samples at room temperature will show obvious insulation decline after moisture absorption. Thermal box tests evaluate the penetration resistance under initial thermal runaway. Impact tests are also necessary, because cracked housings will lose protective functions even if the material itself meets flame retardant standards. All test records should be filed for traceability.

6. Risk Control in Mass Production

Raw materials should be stored in dry warehouses and dried strictly according to specifications. The injection machine and feeding system must be dedicated to prevent cross-contamination with conductive materials. The mold should be cleaned regularly to remove precipitates and carbon deposits. Batch sampling inspection is required to monitor flame retardancy and insulation performance. Many developers only focus on flame retardant grades and ignore CTI and damp heat insulation attenuation, which will cause hidden leakage risks after long-term vehicle operation.